Skip to main content

Kisaju, Kajiado CountyMon – Sat, 8 AM – 5 PM

Materials for furnace, kiln and boiler linings

A lining fails at its weakest layer: a mortar rated below the brick, a hot face too light for the abrasion, or no back-up insulation, leaving the casing too hot to touch. Specify it as a system, from the hot face out.

Layer by layer

Hot face, heavy duty
Firebrick in 40% alumina (1600°C), 70% alumina (1750–1800°C) or zirconia (2000°C); Maxheat A dense castable (1750°C). Firebricks
Hot face, light duty
Ceramic fibre blanket and board (1260 grade); Maxlyte 11 insulating castable (1300°C). Ceramic fibre blanket
Back-up insulation
Insulating brick, about 2 kg each; calcium silicate board (1000°C); vermiculite fill (1100°C). High-temperature boards
Joints
Maxset 50 Fine mortar (1500°C) and Fondu Max-50 calcium aluminate cement. Castables and mortars
Seals
Ceramic fibre rope, tape and cloth, 1260 grade, non-asbestos. Ceramic fibre rope, tape and cloth

Tell us

The hot-face temperature; the fuel and what touches the lining (flame, slag, metal, abrasion); how often it heats and cools; the lining area or a drawing; and whether it is a new lining or a repair.

Request a Material Quotation

We supply the materials; installation and design stay with your contractor or engineer.

Read next

Send us your material list

A specification, a BOQ or a photo of the label on the old stock is enough to start. We reply with an itemised quotation.

Or call or WhatsApp 0722 293 517